p-Toluenesulfonic acid → Propylene glycol methyl ether acetate

https://huagongshe.com/reaction/1425631

Reaction equation

Participants

RoleNameHCIDCharge
Reactantp-Toluenesulfonic acidHCID 6101—
ReactantEthyl vinyl etherHCID 8023—
ReactantEthyl AcetateHCID 8857—
SolventTriethylamineHCID 8471—
ProductPropylene glycol methyl ether acetateHCID 7946—
Productp-1-Ethoxyethoxystyrene p-hydroxystyreneHCID 131719558—

Reaction Steps

Into a 500 ml-volume three-neck flask, 72.1 g of poly-4-hydroxystyrene (VP-8000, produced by Nippon Soda Co., Ltd.), 16.4 g of ethyl vinyl ether and 300 ml of ethyl acetate were charged. A catalytic amount of para-toluenesulfonic acid was added, and reaction was allowed to proceed at room temperature for 3 hours in a nitrogen stream. After adding a small amount of triethylamine, the solution was washed with pure water. Propylene glycol monomethyl ether acetate was added to the ethyl acetate layer, and ethyl acetate was removed by distillation under reduced pressure to obtain Polymer A′-11 (p-1-ethoxyethoxystyrene/p-hydroxystyrene) as a propylene glycol monomethyl ether acetate solution.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS08932800B2
Source datasetuspto-grants-2015_01
ORD IDord-53d1433d1f714253bacbce5b5bf8dd4b