Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1439445Generated: October 31, 2026

Methacrylic Acid → Methacrylic Acid

https://huagongshe.com/reaction/1439445

Reaction equation

Participants

RoleNameHCIDCharge
ReactantMethacrylic AcidHCID 4093—
ReactantHCID 178435178HCID 178435178—
SolventWaterHCID 962—
ProductMethacrylic AcidHCID 4093—
ProductPropyleneHCID 8252—

Reaction Conditions

Temperature95 °C

Reaction Steps

A modified resinous polymer of propylene containing approximately 10% by weight methacrylic acid was prepared as follows: 0.5 grams of Lupersol 256 Peroxide (peroxyhexanoic acid manufactured by Wallace & Tiernan Inc., Lucidol Division) was added to a reactor containing 200 grams of substantially crystalline homopolymeric polypropylene powder, 25 grams of methacrylic acid and 600 grams of water. The mixture was then heated at just below reflux temperature, about 95° C, for one hour. The product was filtered and washed with water followed by acetone and then dried in a vacuum oven at 75° C for two hours. The modified resinous polymer of propylene weighed 225.6 grams.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04059650
Source datasetuspto-grants-1977_11
ORD IDord-3f990c5d523342fa87d8f5d1b833b16e
Source noteuspto-grants-1977_11