HuagongsheHuagongshe Chemistry Print Report · For research reference only
Toluene 2,4-Diisocyanate → Urethane acrylate
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Toluene 2,4-Diisocyanate | HCID 11443 | — |
| Reactant | 2-Hydroxyethyl acrylate | HCID 13165 | — |
| Reactant | 2,6-Di-tert-butyl-4-methylphenol | HCID 31404 | — |
| Reactant | CID 3084433 | HCID 3084433 | — |
| Product | Urethane acrylate | HCID 21863578 | — |
Reaction Steps
To a reaction vessel equipped with a stirrer, 104.3 gm of 2,4-tolylene diisocyanate, 1 gm of dibutyltindilaurate, and 0.3 gm of 2,6-di-t-butyl-4-methylphenol as a polymerization inhibitor were added. To this, 856.0 gm of polytetramethylene glycol of a number average molecular weight of 2,000 (commercial product PTG2000 manufactured by Hodogaya Chemical) was added while maintaining the temperature in the 40° to 50° C. range, and reacted for 2 hours. Next, 2-hydroxyethylacrylate was added, after which the mixture was continuously stirred for 5 hours at 50° to 60° C. to complete the reaction. A urethane acrylate [B-2] of a number of average molecular weight of about 5,840 was obtained.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05496870 |
| Source dataset | uspto-grants-1996_03 |
| ORD ID | ord-24cb1305682c4ca38aebd3f0284cc904 |
| Source note | uspto-grants-1996_03 |