Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1447105Generated: November 3, 2026

Sodium Tripolyphosphate → Pentasodium triphosphate hexahydrate

https://huagongshe.com/reaction/1447105

Reaction equation

Participants

RoleNameHCIDCharge
ReactantSodium TripolyphosphateHCID 24455—
SolventWaterHCID 962—
ProductPentasodium triphosphate hexahydrateHCID 23064738—

Reaction Steps

While the drum was rotating at about 6 rpm, the water was sprayed onto the solids at the rate of about 50 ml/min. Spraying was stopped after each 50 ml portion of water was added and the bed of semi-moisturized sodium tripolyphosphate was thoroughly mixed with a large spatula. When the desired amount of water had been added, water addition was stopped and the product was dried in the rotary drum at temperatures of 50°-70° C. by blowing hot air from a heat gun into the rotary. The temperature of the product being dried was measured by a stainless steel thermometer stem placed in the tumbling bed of product. Drying was conducted for about one hour and generally provided a sodium tripolyphosphate hexahydrate product having a free moisture content of less than about 1 weight percent and a total moisture content of between 18 and 22 weight percent.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04315898
Source datasetuspto-grants-1982_02
ORD IDord-7bad8b82b66346d480649e5c185fe4b1
Source noteuspto-grants-1982_02