Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1447713Generated: October 28, 2026

Pentachlorophenol → HCID 86733443, compound

https://huagongshe.com/reaction/1447713

Reaction equation

Participants

RoleNameHCIDCharge
ReactantPentachlorophenolHCID 992—
ReactantPropylene OxideHCID 6378—
ReactantTriphenyl phosphiteHCID 7540—
ReactantPentaerythritolHCID 8285—
ReactantTriethyl phosphiteHCID 31215—
ReactantAluminumHCID 5359268—
CatalystIronHCID 23925—
ProductHCID 86733443HCID 86733443—

Reaction Conditions

Temperature80 °C

Reaction Steps

A 5-liter flask, standardly equipped, was charged with 1596 grams of pentachlorophenol containing about 750 ppm of aluminum and iron compounds, 680 grams of pentaerythritol and a mixture of 195 grams of triethylphosphite and 260 grams of triphenylphosphite that had been heated overnight at 80° C. Then propylene oxide was added until the acid number was less than 1. The mixture was stripped for 2 hours at 90°-104° C./2-4 mm. Hg. The 3562 grams of oxypropylated polyol product contained a finely divided solid. Upon filtering and washing thoroughly with acetone, approximately 75 grams of the dried solid material was obtained. A sample of the oxypropylated polyol product analyzed as follows:

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04177335
Source datasetuspto-grants-1979_12
ORD IDord-4e81d660eddc4241805d4b565ef8eff1
Source noteuspto-grants-1979_12