Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Pentachlorophenol | HCID 992 | — |
| Reactant | Aniline | HCID 6115 | — |
| Reactant | Propylene Oxide | HCID 6378 | — |
| Reactant | Triphenyl phosphite | HCID 7540 | — |
| Reactant | Aluminum | HCID 5359268 | — |
| Catalyst | Iron | HCID 23925 | — |
| Solvent | Triethylamine | HCID 8471 | — |
| Product | HCID 86733445 | HCID 86733445 | — |
Reaction Steps
A 5-liter flask, standardly equipped, was charged with 1330 grams of pentachlorophenol containing about 750 ppm of aluminum and iron compounds, 500 grams of triphenylphosphite and 232.5 grams of aniline. After heating to approximately 125° C., 750 ml. of propylene oxide was added at a temperature up to 150° C. The mixture was then cooled and 35 grams of triethylamine added, followed by oxypropylation at approximately 90° C. until steady refluxing. The product was then stripped for 2 hours at 80°-82° C./1-2 mm. Hg. The 2931 grams of oxypropylated product had the following properties.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04177335 |
|---|
| Source dataset | uspto-grants-1979_12 |
|---|
| ORD ID | ord-fc3762f260594e1a9d2e7349f180a82e |
|---|
| Source note | uspto-grants-1979_12 |
|---|