Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Pentachlorophenol | HCID 992 | — |
| Reactant | Propylene Oxide | HCID 6378 | — |
| Reactant | Triphenyl phosphite | HCID 7540 | — |
| Reactant | Diethanolamine | HCID 8113 | — |
| Reactant | Aluminum | HCID 5359268 | — |
| Product | HCID 86733447 | HCID 86733447 | — |
Reaction Steps
A 1-liter flask, standardly equipped, was charged with 266 grams of pentachlorophenol containing between 700 and 800 parts per million of aluminum and ferric compounds and 80.3 grams of triphenylphosphite, and then 105.4 grams of diethanolamine was added in increments. By the time the addition of the amine was completed, the temperature had risen to 66° C. and the mixture was extemely viscous. By the time the temperature had increased to 90° C. and approximately 50 ml. of propylene oxide had been added the mixture stirred readily and no further difficulty was encountered. After enough propylene oxide had been dded to obtain a low acid number, the product was stripped for three hours at 1-2 mm. Hg from 74°-98° C. to remove volatiles. The oxypropylated product had a viscosity of 9300 cps at 27° C.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04177335 |
|---|
| Source dataset | uspto-grants-1979_12 |
|---|
| ORD ID | ord-caba7ad342e94b6e882bbf486e25309e |
|---|
| Source note | uspto-grants-1979_12 |
|---|