Trimethyl borate → Boric Acid
Reaction equation
[B:1]([O:6][CH3:7])([O:4][CH3:5])[O:2][CH3:3].C(OCCOCCO)(=O)C(C)=C>>[B:1]([OH:6])([OH:4])[OH:2].[B:1]([O:6][CH3:7])([O:4][CH3:5])[O:2][CH3:3]Participants
Conditions
- Temperature
- 60 °C
Procedure
207.6 Grams (2.0 mols) of trimethyl borate was added to 522 g (3.0 mols) of diethylene glycol monomethacrylate. The mixture was heated to 60° C. with stirring in a dry air atmosphere. The mixture was kept at 60° C. for 1 hour, followed by heating to 75° C. After the temperature reached 75° C., the pressure in the system was gradually reduced. The system was kept at a pressure of 2.67 kPa (20 mmHg) or lower for 6 hours to remove volatile matters produced with progress of ester interchange reaction of boric acid and excess trimethyl borate, followed by filtration to obtain 515 g of a polymerizable boron-containing compound H (an esterification product of boric acid with diethylene glycol monomethacrylate) represented by the formula (2). An infrared absorption spectrum of the resulting polymerizable boron-containing compound H was measured to confirm that the absorption band originating from hydroxyl group at 3300 cm−1 disappeared.
Workup
- temperatureby heating to 75° C
- customreached 75° C.
- waitThe system was kept at a pressure of 2.67 kPa (20 mmHg) or lower for 6 hours
- customto remove volatile matters
Sources & evidence
- ORD record
- ord-419e4f71239c4bd7938b7db6d2479101
- Source dataset
- uspto-grants-2009_01
- Patent number
- US07473492B2
Reaction notes
Loading…