Sodium Phosphate, Dibasic → Hydroxylapatite (Ca5(OH)(PO4)3)
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Sodium Phosphate, Dibasic | HCID 24203 | — |
| Reactant | Calcium Chloride | HCID 5284359 | — |
| Product | Hydroxylapatite (Ca5(OH)(PO4)3) | HCID 14781 | — |
Reaction Steps
Brushite was prepared in the same manner as in Example 1 except that 1 l of an aqueous calcium chloride solution of 0.5 mol/l in concentration and 1 l of an aqueous disodium phosphate solution of 0.5 mol/l in concentration were used and reaction temperature was room temperature. Then, at 95° C., 300 ml of an aqueous sodium hydroxide solution of 1 mol/l in concentration was added to the resulting brushite over a period of 1 hour to obtain hydroxylapatite in the form of platy crystal [hereinafter referred to as "hydroxylapatite (H)"].
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05073357 |
| Source dataset | uspto-grants-1991_12 |
| ORD ID | ord-3664f7782a164eccb7ae4d550227b3ea |
| Source note | uspto-grants-1991_12 |