Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | 2,4-Dinitrotoluene | HCID 8461 | — |
| Reactant | 2,6-Dinitrotoluene | HCID 11813 | — |
| Reactant | Ammonium nitrate | HCID 22985 | — |
| Reactant | Aluminum | HCID 5359268 | — |
| Product | 2,3-Dinitrotoluene | HCID 11761 | — |
Reaction Steps
Eighty-five (85) parts of porous prill ammonium nitrate (average particle size, 1.7 mm; oil absorbency, 17%) preheated to 70° C., and 14 parts of a liquid dinitrotoluene mixture which was prepared by mixing 2,4-dinitrotoluene with 2,6-dinitrotoluene and heating at 70° C. were thoroughly mixed using a horizontal kneader equipped with a sigma wing, thereby obtaining a granular explosive of the present invention. After cooling, the granular explosive and 1 part of flake-shaped aluminium (P-0100; manufactured by Toyo Aluminium) were mixed using a horizontal kneader. The thus obtained explosive was recovered from the kneader and packed in a paper shell.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US05675119 |
|---|
| Source dataset | uspto-grants-1997_10 |
|---|
| ORD ID | ord-8993242e9b314d44b75cb6dad7de657b |
|---|
| Source note | uspto-grants-1997_10 |
|---|