Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1489306Generated: October 31, 2026

Styrene → Styrene-butadiene-styrene

https://huagongshe.com/reaction/1489306

Reaction equation

Participants

RoleNameHCIDCharge
ReactantStyreneHCID 7501—
Reactant1,3-ButadieneHCID 7845—
ReactantDibutyltin dichlorideHCID 12688—
Reactant2-Propanol, 2-methyl-, lithium salt (1:1)HCID 23664764—
SolventIsopropanolHCID 3776—
SolventHexaneHCID 8058—
SolventCyclohexaneHCID 8078—
SolventHCID 19351698HCID 19351698—
ProductStyrene-butadiene-styreneHCID 22280236—

Reaction Conditions

Temperature60 °C

Reaction Steps

A styrene-butadiene-styrene block polymer was prepared using the cyclic organomagnesium initiator, SBMG, as follows: To the reactor was charged 1.25 lbs. of 24.8% 1,3-butadiene in technical hexane and 3.1 lbs. of additional hexane, followed by 3.8 mM SBMG in styrene/hexane and 5.7 mM of lithium-t-butoxide in cyclohexane. The reactor was then heated to 60° C. and the reaction allowed to proceed for 4 hours. Then 180 grams of 33% styrene in hexane were added and polymerization proceeded for an additional hour. The coupling/functionalizing agent, 3.0 mM of dibutyl-tin-dichloride, was then added to the reactor. After one hour, the resulting polymer cement was isolated by coagulation in an equal volume of isopropanol containing BHT.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05677399
Source datasetuspto-grants-1997_10
ORD IDord-b9049415fc854b849ac9449238a0a269
Source noteuspto-grants-1997_10