Styrene → 2-Methylbuta-1,3-diene;styrene

https://huagongshe.com/reaction/1489311

Reaction equation

Participants

RoleNameHCIDCharge
ReactantStyreneHCID 7501—
ReactantButyllithiumHCID 178418339—
Product2-Methylbuta-1,3-diene;styreneHCID 159989—

Reaction Steps

The procedure described in Example 9 was utilized in this example except that a premix containing 25:75 mixture of styrene and 1,3-isoprene in hexanes was used in place of isoprene and the modifier was changed from STA/DPE to ETE alone. The molar ratio of ETE to n-BuLi was 0.5:1. The Tg, microstructure of 25/75 SIR (styrene-isoprene rubber) formed and the time needed to consume more than 90 percent of the monomers charged are listed in TABLE 8.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05677402
Source datasetuspto-grants-1997_10
ORD IDord-5c58d4b254b4477fb2fd3bb2940dc2e0
Source noteuspto-grants-1997_10