Methacrylic Acid → Methacrylic acid ethylene oxide

https://huagongshe.com/reaction/1499666

Reaction equation

Participants

RoleNameHCIDCharge
ReactantMethacrylic AcidHCID 4093—
ReactantEthylene OxideHCID 6354—
ReactantStyreneHCID 7501—
ReactantAmmonium PersulfateHCID 62648—
ReactantSodiumHCID 5360545—
SolventWaterHCID 962—
ProductMethacrylic acid ethylene oxideHCID 21880491—
ProductStyrene-methacrylic acid sodiumHCID 86592924—

Reaction Conditions

Temperature75 °C

Reaction Steps

A reaction container equipped with a stirring rod and a thermometer was charged with 683 parts by mass of water, 11 parts by mass of sodium salt of sulfuric acid ester of ethylene oxide adduct of methacrylic acid (ELEMINOL RS-30, product of Sanyo Chemical Industries Ltd.), 138 parts by mass of styrene, 138 parts by mass of methacrylic acid and 1 part by mass of ammonium persulfate. The resultant mixture was stirred at 400 rpm for 15 min to thereby obtain a white emulsion. The white emulsion was heated to a system temperature of 75° C. and was allowed to react for 5 hours. Then, 30 parts by mass of a 1% by mass aqueous ammonium persulfate solution was added to the reaction mixture, followed by aging at 75° C. for 5 hours, to thereby obtain an aqueous dispersion [particle dispersion liquid 1] of a vinyl resin (a copolymer of styrene-methacrylic acid-sodium salt of sulfate ester of methacrylic acid-ethylene oxide adduct).

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS09201326B2
Source datasetuspto-grants-2015_12
ORD IDord-e614ed9219c146b6990e56b314b01ef3
Source noteuspto-grants-2015_12