Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Phenol | HCID 996 | — |
| Reactant | Trimellitic anhydride | HCID 11089 | — |
| Product | Adipic Acid | HCID 196 | 59.2% |
Reaction Steps
A solution is formed by mixing 60.0 grams of trimellitic acid anhydride and 130.0 grams of p,p' diphenyl methane diisocyanate and 110.0 grams of Bis 2-ethoxy ethylether and 4.8 grams of phenol by heating the mixture. At approximately 135°C. a clear, homogeneous solution is obtained. Once clarity is obtained 27.0 grams of adipic acid is added slowly. The temperature of the mixture is raised to approximately 190°C. and slow reflux is maintained. After approximately 45 minutes, a brownish viscous resin is obtained and 346.2 grams of phenol are added to quench and stop the reaction. The solution is maintained at 130°C. until all the resin is dissolved. The resultant solution is cooled to room temperature and filtered. The viscosity of the product at 25°C. was measured at about 210 cps, utilizing a Brookfield viscometer, and a resin solution of approximately 30% weight resin.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US03937673 |
|---|
| Source dataset | uspto-grants-1976_02 |
|---|
| ORD ID | ord-3d92eaf1c9bd48e485dfd969161f4524 |
|---|
| Source note | uspto-grants-1976_02 |
|---|