p-Toluenesulfonic acid → HCID 70100107, compound

https://huagongshe.com/reaction/1581907

Reaction equation

Participants

RoleNameHCIDCharge
Reactantp-Toluenesulfonic acidHCID 6101—
ReactantVinyl isobutyl etherHCID 7992—
ReactantTriethylamineHCID 8471—
ReactantEthyl AcetateHCID 8857—
Solvent1-Ethoxypropan-2-yl acetateHCID 171378—
ProductHCID 70100107HCID 70100107—

Reaction Conditions

Temperature60 °C

Reaction Steps

The above polymer (A-48) (20 g) was dissolved in 80 g of propylene glycol monoethyl ether acetate (PGMEA) and the solution was heated at 60° C., and then the pressure was gradually reduced until 20 mmHg, thereby PGMEA and the moisture in the reaction system were azeotropically hydrated. After the azeotropic hydration, the temperature was lowered to 20° C., 2.2 g of isobutyl vinyl ether was added thereto, and further 3 mg of p-toluenesulfonic acid was added. After the addition, reaction was performed for 2 hours, and a small amount of triethylamine was added to neutralize the acid. Thereafter, ethyl acetate was added to the reaction solution, and the salt was removed by washing with ion exchange water. Further, ethyl acetate and water were distilled off under reduced pressure, thereby polymer A-16 was obtained.

Provenance & Evidence