HuagongsheHuagongshe Chemie-Druckbericht · Nur für Forschungszwecke
Methanol → Isooctylacrylate Acrylamide
Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|---|---|---|
| Edukt | Methanol | HCID 887 | — |
| Edukt | Acrylamide | HCID 6579 | — |
| Edukt | Benzoyl Peroxide | HCID 7187 | — |
| Edukt | Isooctyl acrylate | HCID 165746 | — |
| Lösungsmittel | Ethyl Acetate | HCID 8857 | — |
| Lösungsmittel | Ethylacetate methanol | HCID 21584119 | — |
| Produkt | Isooctylacrylate Acrylamide | HCID 6452299 | — |
Reaktionsschritte
To a quart narrow-mouth glass bottle were added: 127.84 g. isooctyl acrylate, 8.6 g. acrylamide, 0.41 g. benzoyl peroxide, 237.6 g. ethyl acetate and 26.4 g. methyl alcohol. The solution was purged for two minutes with nitrogen at a flow rate of one liter per minute. The bottle was sealed and placed in a rotating water bath at 55° C. for twenty four hours to effect essentially complete polymerization. The polymer was diluted with ethyl acetate/methyl alcohol (90/10) to 28.4% solids and had a measured inherent viscosity of 1.02 dl/g. in ethyl acetate at a concentration of 0.15 g/dl. Its Brookfield viscosity was 9,120 centipoise.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patentnummer | US05223261 |
| Quelldatensatz | uspto-grants-1993_06 |
| ORD ID | ord-95991d802a2243008a8b0a568a0b2523 |
| Quellennotiz | uspto-grants-1993_06 |