참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Tetrahydrofuran | HCID 8028 | — |
| 촉매 | 12-Wolframophosphoric acid | HCID 452313 | — |
| 용매 | Water | HCID 962 | — |
| 생성물 | CID 3084433 | HCID 3084433 | — |
반응 단계
Polymerization was carried out by means of the continuous polymerization device as shown in FIGURE. First, into a polymerization tank 1 of 350 ml volume equipped with a stirrer and a reflux condenser, 135 g of phosphotungstic acid with a coordinated water molecules number of 3.3 (H3PW12O40.3.3H2O) was charged and 270 g of THF with a water content of 200 ppm was added, followed by stirring. The polymerization tank was set at a temperature of 60° C. and THF containing water of 0.4 wt. % was fed at a rate of 60 g/hour. The polymerization tank mixture was circulated between the tank and the phase separation tank 2, and the upper layer separated was withdrawn at a rate of 60 g/hour. From the upper layer, THF was removed by distillation, resulting to provide PTMG. After continuous running for 260 hours, 2.0 Kg of a PTMG with a number-average molecular weight of 1750 was obtained.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US04568775 |
|---|
| 출처 데이터셋 | uspto-grants-1986_02 |
|---|
| ORD ID | ord-7b39fb76d99f4216a1c7ec010fe6c087 |
|---|
| 출처 메모 | uspto-grants-1986_02 |
|---|