Ammonia → HCID 87324800, compound
Reaction equation
[NH3:1].[CH3:2][C:3](=[CH2:5])[CH3:4].[C:6]1(=[O:12])[O:11][C:9](=[O:10])[CH:8]=[CH:7]1.C=CC(=C)C>>[CH3:4][C:3](=[CH2:2])[CH3:5].[C:6]1(=[O:12])[NH:1][C:9](=[O:10])[CH:8]=[CH:7]1.[C:9]1(=[O:10])[O:11][C:6](=[O:12])[CH:7]=[CH:8]1Participants
4
Conditions
- Temperature
- 180 °C
Procedure
In an ammonia gas atmosphere, 100 parts of an isobutylene-maleic anhydride copolymer (sold under the trade name "ISOBAN 04" by KURARAY ISOPRENE K.K. of Kita-ku, Osaka, Japan) was heated to 180° C. to obtain an isobutylene-maleic imide-maleic anhydride copolymer. Then placed in a reactor were 40 parts of the isobutylene-maleic imide-maleic anhydride copolymer, 7 parts of 25% ammonia water and 160 parts of water. The mixture in the reactor was heated at 85° C. for 2 hours, thereby obtaining an aqueous solution of isobutylene-maleic imide-maleic anhydride copolymer. The aqueous solution contained 20% nonvolatile matter, and the viscosity of the aqueous solution was measured at 6,000 mPa.s.
Sources & evidence
- ORD record
- ord-c0830a8256bb4663be07dbb50d7f86aa
- Source dataset
- uspto-grants-1999_11
- Patent number
- US05977242
Reaction notes
Loading…