Styrene → Benzene, ethenyl-, polymer with 1,3-butadiene

HRID 1606226Notes

Reaction equation

HRID 1606226 reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1>C1C=CC=CC=1>[CH2:1]=[CH:2][CH:3]=[CH2:4].[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1

Participants

3

Procedure

To 15g. of styrene placed in a tube is added 5g. of the product obtained in Example III. The tube is sealed under a nitrogen atmosphere and heated for seven hours at +70°C to +100°C. The polymer obtained from the reaction is dissolved in benzene and precipitated with odorless mineral spirit. The polymer is dried in a vacuum oven for 16 hours at +50°C and tested by the demixing test. (4)-(5).

Workup

  1. customThe tube is sealed under a nitrogen atmosphere
  2. temperatureheated for seven hours at +70°C to +100°C
  3. customThe polymer obtained from the reaction
  4. customprecipitated with odorless mineral spirit
  5. customThe polymer is dried in a vacuum oven for 16 hours at +50°C