Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Phenol | HCID 996 | — |
| Reactant | Aluminum | HCID 5359268 | — |
| Product | Phenol, aluminum salt (3:1) | HCID 167236 | — |
Reaction Steps
In a reaction vessel was placed 8100 parts of phenol and 27 parts of aluminum metal. The vessel was sealed and heated to 150° C. to form aluminum triphenoxide. This catalyst concentrate was then mixed with 11,124 parts of additional phenol. This gives a phenol/aluminum mole ratio of about 203. The phenolcatalyst mixture was cooled to 90° C. and 23,490 parts of isobutylene was pumped in over a 50-minute period. The reaction temperature rose to 110° during the first 10 minutes of isobutylene feed. Stirring was continued at 110°-115° C. for 165 minutes. Reactor pressure dropped to 120 psig from a maximum of 260 psig.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04870216 |
|---|
| Source dataset | uspto-grants-1989_09 |
|---|
| ORD ID | ord-d3df0efde2284c86b383f7cb61d8aaa0 |
|---|
| Source note | uspto-grants-1989_09 |
|---|