HuagongsheHuagongshe Chemistry Print Report · For research reference only
Ethylene Oxide → HCID 131717461, compound
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Ethylene Oxide | HCID 6354 | — |
| Reactant | Sodium Hydroxide | HCID 14798 | — |
| Reactant | Sodium Azide | HCID 33557 | — |
| Reactant | 2-(Chloromethyl)oxirane--oxirane (1/1) | HCID 168228 | — |
| Reactant | HCID 513618 | HCID 513618 | — |
| Solvent | Dimethylacetamide | HCID 31374 | — |
| Product | HCID 131717461 | HCID 131717461 | — |
Reaction Steps
Elastomeric GEC is prepared according to the same previous procedure as in Example 1, except that commercial rubbery Epichlorohydrin-Ethylene Oxide Copolymer (PEEC) is used instead of PECH as the starting material. The copolymer contains about 70% PECH and 30% Ethylene Oxide. For this reason, a weight ratio NaN3 :PEEC of 0.55 is used in this case. Specifically, the reaction for 16 h at 100° C. of 10 g PEEC (MW~9×105) in 50 g DMA and 5 g EG with 5.5 g NaN3 and 1.5 g NaOH will yield 9.0 g (90%) of GEC azido product. This copolymer containing about 70% GAP and 30% Ethylene Oxide has a MW of about 10,000, a Tg of about -55° C. and a functionality (f) of about 3.5.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05191034 |
| Source dataset | uspto-grants-1993_03 |
| ORD ID | ord-46d33a1fb89f457c8ec1bf2eedfc697a |
| Source note | uspto-grants-1993_03 |