Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1613531Generated: November 2, 2026

Acrylic Acid → Acrylic Acid

https://huagongshe.com/reaction/1613531

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAcrylic AcidHCID 6581—
ReactantMaleic AnhydrideHCID 7923—
ReactantPotassium PersulfateHCID 24412—
ReactantSodiumHCID 5360545—
ReactantHCID 178418950HCID 178418950—
ReactantHCID 178527019HCID 178527019—
SolventWaterHCID 962—
ProductAcrylic AcidHCID 6581—
ProductMaleic AcidHCID 444266—

Reaction Steps

Copolymers of acrylic acid and maleic acid were prepared using sodium hypophosphite to promote telomerization. In a typical reaction, sodium hypophosphite monohydrate of a desired amount was added to deionized water and the solution heated to about 90°-100° C. Maleic anhydride was added to the solution and pH adjusted to about 4. Sodium or potassium persulfate (1-10% of total monomer feed) was used to initiate the polymerization. Acrylic acid at the appropriate ratio was added periodically over a 2-4 hour time period. Polymerization was continued until substantially 100% conversion was obtained. Telomers prepared in this manner are listed in Table I.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05194246
Source datasetuspto-grants-1993_03
ORD IDord-bec6657ee9fb4441b5e08853d9e69829
Source noteuspto-grants-1993_03