HuagongsheHuagongshe Chemistry Print Report · For research reference only
Potassium Carbonate → Carbon Dioxide
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Potassium Carbonate | HCID 11430 | — |
| Solvent | Water | HCID 962 | — |
| Product | Carbon Dioxide | HCID 280 | — |
| Product | Potassium Carbonate | HCID 11430 | — |
Reaction Steps
Heating a slurry with the initial composition of 50 ml water, 38.18 g KHCO3, and 23.65 g K2CO3 at 125.8° C. and 1.6 atm. produced 37.27 g K2CO3 and 11.87 g CO2, and the pH in the solution was 11.6. The total energy demand was estimated to be 2683 kJ/kg CO2, including 1014 sensible heat, 190 latent heat, and 1479 enthalpy.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US08771403B2 |
| Source dataset | uspto-grants-2014_07 |
| ORD ID | ord-2408ba7e2ebb41fc9a219c0f39c9304d |
| Source note | uspto-grants-2014_07 |