HuagongsheHuagongshe Chemistry Print Report · For research reference only
Potassium Carbonate → Carbon Dioxide
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Potassium Carbonate | HCID 11430 | — |
| Solvent | Water | HCID 962 | — |
| Product | Carbon Dioxide | HCID 280 | — |
| Product | Potassium Carbonate | HCID 11430 | — |
Reaction Steps
Heating a slurry with the initial composition of 50 ml water, 38.18 g KHCO3, and 23.65 g K2CO3 at 125.5° C. and 1.8 atm. produced 33.67 g K2CO3 and 10.72 g CO2, and the pH in the solution was 11.35. The total energy demand was estimated to be 2808 kJ/kg CO2, including 1119 sensible heat, 210 latent heat, and 1479 enthalpy.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US08771403B2 |
| Source dataset | uspto-grants-2014_07 |
| ORD ID | ord-92aa978047e4428190e0a06da0f2a419 |
| Source note | uspto-grants-2014_07 |