Azobisisobutyronitrile → Styrol-acryl-nitril

https://huagongshe.com/reaction/1620354

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAzobisisobutyronitrileHCID 6547—
ReactantStyreneHCID 7501—
ReactantAcrylonitrileHCID 7855—
ReactantTricalcium PhosphateHCID 24456—
SolventWaterHCID 962—
ProductStyrol-acryl-nitrilHCID 279762—

Reaction Steps

76 parts by weight of styrene, 24 parts by weight of acrylonitrile, and 120 parts of deionized water are mixed. To the mixture, 0.17 parts by weight of azobisisobutylonitrile (AIBN), 0.4 parts by weight of t-dodecyl mercaptan chain transfer agent, and 0.5 parts by weight of tricalciumphosphate are added. The mixture is suspension polymerized at 75° C. for 5 hours, and a styrene-acrylonitrile (SAN) copolymer resin is obtained. The resultant copolymer is washed, dehydrated and dried to obtain SAN copolymer resin having a weight average molecular weight of 150,000 g/mol in powder form.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS08772401B2
Source datasetuspto-grants-2014_07
ORD IDord-c580d4a94860445c8ed08c3cf458a254
Source noteuspto-grants-2014_07