Aluminum(III) Chloride → HCID 13339632, compound
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Aluminum(III) Chloride | HCID 6451240 | — |
| Reactant | HCID 20443326 | HCID 20443326 | — |
| Solvent | Carbon Tetrachloride | HCID 5943 | — |
| Product | HCID 13339632 | HCID 13339632 | 80% |
Reaction Steps
To a slurry of 5 g of neutral alumina in 300 ml of carbon tetrachloride was added 0.5 g of anhydrous aluminum chloride and the mixture was heated at reflux for 20 minutes. To the slurry was added 20 g (0.052 mole) of 2,3-dichloro-5-(1-bromo-3,3,3-trichloro-1-methylpropyl)pyridine, and the resulting mixture was heated at reflux for 48 hours. The mixture was cooled and filtered. The filtrate was concentrated in vacuo yielding the crude product. Recrystallization from pentane yielded 12.7 g (80%) of product, m.p. 76°-77° C.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04474602 |
| Source dataset | uspto-grants-1984_10 |
| ORD ID | ord-ab4311dbae0d46b398d842db1e42dc15 |
| Source note | uspto-grants-1984_10 |