Alpha-Methylstyrene → Acrylonitrile alpha-methylstyrene

https://huagongshe.com/reaction/1647257

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAlpha-MethylstyreneHCID 7407—
ReactantAcrylonitrileHCID 7855—
ReactantPotassium PersulfateHCID 24412—
ReactantSodium Lauryl SulfateHCID 3423265—
SolventWaterHCID 962—
ProductAcrylonitrile alpha-methylstyreneHCID 168415—

Reaction Conditions

Temperature70 °C

Reaction Steps

In a reactor which had been replaced with nitrogen, pure water (150 parts), potassium persulfate (0.5 part) and sodium laurylsulfate (2 parts) were charged and heated to 70° C. while stirring. Then, a mixed monomer solution of acrylonitrile (30 parts), α-methylstyrene (70 parts) and tert.-dodecylmercaptan (0.2 part) was continuously added over 5 hours. The polymerization system was heated to 75° C. and aged for 5 hours to complete the polymerization to obtain a latex of acrylonitrile-α-methylstyrene copolymer.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05430101
Source datasetuspto-grants-1995_07
ORD IDord-772e3ba7a9b74d24823dec19bd6539bc