Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Quinone | HCID 4650 | — |
| Reactant | Ethylene | HCID 6325 | — |
| Reactant | 1-Dodecene | HCID 8183 | — |
| Reactant | 1,3-Bis(diphenylphosphino)propane | HCID 81219 | — |
| Reactant | HCID 178418416 | HCID 178418416 | — |
| Catalyst | palladium(II) acetate | HCID 167845 | — |
| Solvent | Methanol | HCID 887 | — |
| Product | HCID 178443135 | HCID 178443135 | — |
Reaction Steps
A carbon monoxide/ethylene/1-dodecene terpolymer was prepared by charging 180 ml of methanol and 78 ml of 1-dodecene to a magnetically stirred autoclave of 300 ml capacity. After the contents of the autoclave had been heated to 65° C., a 1:1 carbon monoxide and ethylene mixture was introduced under pressure until a pressure of 55 bar was reached. A catalyst solution was then introduced comprising 18 ml of methanol, 0.03 mmol of palladium acetate, 0.06 mmol of copper para-tosylate, 0.036 mmol of 1,3-bis(diphenylphosphino)propane, and 0.3 mmol of 1,4-benzoquinone. The pressure in the autoclave was maintained by introducing additional amounts of the 1:1 carbon monoxide and ethylene mixture. After 3 hours the polymerization was terminated by cooling to room temperature and releasing pressure. The polymer was filtered, washed with methanol and dried at 70° C.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04921937 |
|---|
| Source dataset | uspto-grants-1990_05 |
|---|
| ORD ID | ord-2dcf6ae365284643841cf4ccd7fa31f6 |
|---|
| Source note | uspto-grants-1990_05 |
|---|