Dimethyladipate → HCID 131715825, compound
Reaction equation
[C:1]([O:11]C)(=[O:10])[CH2:2][CH2:3][CH2:4][CH2:5][C:6]([O:8]C)=[O:7].[CH3:13][O:14][C:15]1[CH:20]=[CH:19][C:18]([CH2:21][N:22]2[CH2:27][CH2:26][N:25]([CH2:28][C:29]3[CH:34]=[CH:33][CH:32]=[CH:31][CH:30]=3)[CH2:24][CH2:23]2)=[C:17]([OH:35])[C:16]=1[O:36][CH3:37].C([Sn](=O)CCCC)CCC>CO>[CH3:13][O:14][C:15]1[CH:20]=[CH:19][C:18]([CH2:21][N:22]2[CH2:23][CH2:24][N:25]([CH2:28][C:29]3[CH:30]=[CH:31][CH:32]=[CH:33][CH:34]=3)[CH2:26][CH2:27]2)=[C:17]([OH:35])[C:16]=1[O:36][CH3:37].[C:1]([O-:11])(=[O:10])[CH2:2][CH2:3][CH2:4][CH2:5][C:6]([O-:8])=[O:7]Participants
5
Reactant 3
Product 1
Reagents, catalysts & solvents 1
Conditions
- Temperature
- 180 °C
Procedure
Into the resin cook apparatus described in Example 1 are charged dimethyl adipate (200 grams, 1.15 moles), BHDP (302 grams, 1.37 moles), and dibutyltin oxide (1.0 gram). The mixture is heated at 180° C. for 4 hours. A conversion of 93 percent is obtained based upon the methanol taken overhead. The tacky polyester has an average molecular weight of 1,974, an acid number of 2.4, and a hydroxyl number of 50.0.
Workup
- customA conversion of 93 percent is obtained
Sources & evidence
- ORD record
- ord-1d653c2acdf74da99ed5c6e045574dd2
- Source dataset
- uspto-grants-1990_05
- Patent number
- US04927878