Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1651739Generated: October 30, 2026

Acrylamide → HCID 131716395, compound

https://huagongshe.com/reaction/1651739

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAcrylamideHCID 6579—
ReactantHeptaneHCID 8900—
ReactantChlorineHCID 24526—
Reactant19895-66-0HCID 29853—
SolventEthanolHCID 702—
SolventWaterHCID 962—
ProductHCID 131716395HCID 131716395—

Reaction Conditions

Temperature0 °C

Reaction Steps

A 20% solids copolymer of acrylamide-DADM of molecular weight of 180,000 is prepared by polymerization of 75 wt % of acrylamide and 25 wt % of DADM. 50 parts of the copolymer is diluted with 150 parts of water in the reaction flask. 150 Parts of n-heptane are added and the mixture is stirred and cooled externally to 0° C. 1598 c.c. of chlorine are charged into the reaction mixture in 15 minutes while the temperature of the reaction mixture is kept at 0° C. to 2° C. during the chlorination process by external cooling. The reaction mixture is then poured slowly into 2 liters of ethanol with agitation. The product polymer is precipitated. The precipitate is collected by filtration and dried. It is found by analysis that the product polymer contains 26.2 mole % of N-chloroamide units.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04929687
Source datasetuspto-grants-1990_05
ORD IDord-00390ec6dbc14c49a8a9c59354500f42
Source noteuspto-grants-1990_05