HuagongsheHuagongshe Chemistry Print Report · For research reference only
Methanol → HCID 86733590, compound
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Methanol | HCID 887 | — |
| Reactant | Triphenylphosphine | HCID 11776 | — |
| Reactant | Rhodium chloride | HCID 24872 | — |
| Reactant | Sodium borohydride | HCID 4311764 | — |
| Reactant | HCID 178418361 | HCID 178418361 | — |
| Reactant | HCID 178418416 | HCID 178418416 | — |
| Solvent | Water | HCID 962 | — |
| Product | HCID 86733590 | HCID 86733590 | — |
Reaction Steps
The catalyst was also prepared from rhodium trichloride by the addition of one gram hydrated rhodium trichloride to 200 milliliters methanol and 20 milliliters water. To the mixture was added 7 grams of triphenylphosphine and the system was then refluxed for 30 minutes under an atmosphere containing equal molar quantities of carbon monoxide and hydrogen. Thereafer 2 grams of sodium borohydride dissolved in 50 milliliters of methanol were added and the system was refluxed for another 30 minutes, then cooled and filtered. The yellow solid was washed thoroughly with metahnol and air dried to obtain 3.49 grams of tris(triphenylphosphine rhodium carbonyl hydride.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US03965192 |
| Source dataset | uspto-grants-1976_06 |
| ORD ID | ord-28e5082a78f3446db1cc4dac0555aaa7 |
| Source note | uspto-grants-1976_06 |