Styrene → Benzene, ethenyl-, polymer with 1,3-butadiene

HRID 1659603Notes

Reaction equation

HRID 1659603 reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1>C1C=CC=CC=1>[CH2:1]=[CH:2][CH:3]=[CH2:4].[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1

Participants

3

Procedure

To 15 g. of styrene placed in a tube is added 5 g. of the product obtained on Example V. The tube is sealed under a nitrogen atmosphere and heated for seven hours at +70° C. to +100° C. The polymer obtained from the reaction is dissolved in benzene and precipitated with odorless mineral spirit. The polymer is dried in a vacuum oven for sixteen hours at +50° C. and tested by the demixing test. (4)-(5).

Workup

  1. additionis added 5 g
  2. customof the product obtained on Example V
  3. customThe tube is sealed under a nitrogen atmosphere
  4. temperatureheated for seven hours at +70° C. to +100° C
  5. customThe polymer obtained from the reaction
  6. customprecipitated with odorless mineral spirit
  7. customThe polymer is dried in a vacuum oven for sixteen hours at +50° C.