HuagongsheHuagongshe Chemistry Print Report · For research reference only
Acrylamide → Acrylamide 2-Acrylamido-2-Methyl Propyl Sulfonic Acid
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Acrylamide | HCID 6579 | — |
| Reactant | Sodium Hydroxide | HCID 14798 | — |
| Reactant | tert-BUTYL PEROXYPIVALATE | HCID 61238 | — |
| Reactant | 2-Acrylamido-2-methyl-1-propanesulfonic acid | HCID 65360 | — |
| Solvent | Water | HCID 962 | — |
| Product | Acrylamide 2-Acrylamido-2-Methyl Propyl Sulfonic Acid | HCID 86735510 | — |
Reaction Steps
Borax (0.6 g.) and 50% aqueous sodium hydroxide (7.2 g.) were dissolved in 52.4 g. of distilled water. 2-acrylamido-2-methyl propyl sulfonic acid (2-AMPSA) (20.4 g.) and acrylamide (AM) (39.4 g.) were dissolved in the caustic solution while maintaining the temperature at <20° C. by cooling. The pH of the final solution was adjusted to 8.0; the solution was then combined with Tween 85 (30.0 g.) and Mentor 28 (50.0 g.). The reaction was conducted according to the procedure of Example 31. 0.5 ml of a 0.01% FAS solution and 0.1 ml of Lupersol 11 was used; polymerization was maintained at <68° C. by cooling. The product was a stable emulsion (5000 cps viscosity).
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04077930 |
| Source dataset | uspto-grants-1978_03 |
| ORD ID | ord-4014018ffa2843df9842ece71445aa04 |
| Source note | uspto-grants-1978_03 |