Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Propylene Glycol | HCID 1030 | — |
| Reactant | 2-Hydroxyethyl Methacrylate | HCID 13360 | — |
| Reactant | Di-n-butyldilauryltin | HCID 9809426 | — |
| Reactant | Benzylbenzene diisocyanate | HCID 19824838 | — |
| Product | Urethane methacrylate | HCID 10012418 | — |
Reaction Steps
In a 3 L four-necked flask equipped with a stirrer, a reflux condenser tube, a gas introducing pipe, and a thermometer, 500 g of diphenylmethane diisocyanate, 76 g of propylene glycol, and 0.5 g of dibutyltin dilaurate were placed. The mixture was reacted while being stirred at 60° C. for 4 hours. Subsequently, the reactant was stirred while 260 g of 2-hydroxyethyl methacrylate was added dropwise over 2 hours. After the completion of the dropwise addition, the resultant was reacted by stirring for 5 hours to obtain urethane methacrylate. Subsequently, to the urethane methacrylate, 560 g of styrene monomer was added to obtain a urethane methacrylate resin (U-6). The weight average molecular weight of the urethane methacrylate resin (U-6) was 1,403.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08148469B2 |
|---|
| Source dataset | uspto-grants-2012_04 |
|---|
| ORD ID | ord-911b90e0bb404e0e9c4f538c57fe6ba6 |
|---|
| Source note | uspto-grants-2012_04 |
|---|