Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1701261Generated: November 4, 2026

Acrylamide → Acrylamide

https://huagongshe.com/reaction/1701261

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAcrylamideHCID 6579—
ReactantAcrylic AcidHCID 6581—
ReactantPotassium HydroxideHCID 14797—
ProductAcrylamideHCID 6579—
ProductPotassium acrylateHCID 4429391—

Reaction Steps

A 34 gallon batch of a 19 weight percent potassium acrylate and 35 weight percent aqueous acrylamide solution was prepared as follows: 219 pounds of a 50 weight percent acrylamide solution was contacted with 38.4 pounds of acrylic acid, followed by the controlled addition of 58.2 pounds of a 50 percent by weight potassium hydroxide solution, 9.8 pounds of high molecular weight poly (acrylamide), P-250 (commercially available from American Cyanamid, Wayne, New Jersey 07470) in powder form was added in a controlled fashion to the aqueous solution to ensure that the powder was properly dispersed. The concentration of powdered polymer was 3 percent by weight. The thickened solution was mixed in a 100 gallon stainless steel tank with a mechanical stirrer at 48 RPM for 20 hours and remained unagitated for two additional days. Then its viscosity was measured using a Brookfield Viscometer and found to be 43,000 centipoise.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04192727
Source datasetuspto-grants-1980_03
ORD IDord-46d6431fa9a0471fb391ded2a5910f9f
Source noteuspto-grants-1980_03