Isopentane → tert-Butyl peroxybenzoate
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Isopentane | HCID 6556 | — |
| Reactant | Styrene | HCID 7501 | — |
| Reactant | Pentane | HCID 8003 | — |
| Reactant | Potassium Persulfate | HCID 24412 | — |
| Reactant | Tricalcium Phosphate | HCID 24456 | — |
| Solvent | Water | HCID 962 | — |
| Product | tert-Butyl peroxybenzoate | HCID 11966 | — |
Reaction Steps
After having closed the vessel, the mixture was polymerized with agitation for 6.5 hours at 363 K and for 3 hours at 393 K. After a conversion of about 40 to 47% of styrene was achieved, 1.275 g of potassium peroxodisulfate in 100 ml of water and 298 g of tricalcium phosphate in 3 liters of water were added. After 4 hours at 363 K, 5.9 kg of an expanding agent mixture consisting of 75% by weight of n-pentane and 25% by weight of isopentane was forced into the vessel within 15 to 20 minutes.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04192922 |
| Source dataset | uspto-grants-1980_03 |
| ORD ID | ord-9eaaaee21ff04638a655cbb79e2ddef5 |
| Source note | uspto-grants-1980_03 |