Adipic Acid → HCID 86738144, compound

https://huagongshe.com/reaction/1703069

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAdipic AcidHCID 196—
ReactantVinyl ChlorideHCID 6338—
ReactantBenzoyl PeroxideHCID 7187—
ReactantSodium orthosilicateHCID 26051—
ReactantSodium StearateHCID 2724691—
ProductHCID 86738144HCID 86738144—

Reaction Conditions

Temperature50 °C

Reaction Steps

About 50 parts by weight of an aqueous sodium silicate solution containing about 15% Na2O and 25% SiO2 by weight, 2 parts by weight of adipic acid, 0.2 parts by weight of sodium stearate and 0.1 part by weight of benzoyl peroxide are mixed then added to an autoclave and a temperature of about 50° C. is maintained at a pressure between 7.0 and 7.1 kg per cm2. Vinyl chloride monomer is slowly added while agitating over a period of 7 to 10 hours until the emulsion contains about 30% vinyl chloride polymerized with the sodium silicate thereby producing an emulsion of poly(sodium silicate-vinyl chloride) copolymer.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04350775
Source datasetuspto-grants-1982_09
ORD IDord-b78da6b73abc40bb920c7932b4b7b627