Reactant4-Aminobenzoic AcidHCID 978—
ReactantVinylidene chlorideHCID 6366—
ReactantBenzoyl PeroxideHCID 7187—
ReactantDiacetyl peroxideHCID 8040—
ReactantSodium orthosilicateHCID 26051—
ReactantSodium Lauryl SulfateHCID 3423265—
ProductHCID 86738145HCID 86738145—

Reaction Steps

About 50 parts by weight of an aqueous sodium silicate solution containing about 14.7% Na2O and 29.4% SiO2 by weight, 2 parts by weight of para-aminobenzoic acid, 0.5 parts by weight of sodium lauryl sulphate, 0.05 parts by weight acetyl peroxide, 0.05 parts by weight of benzoyl peroxide and 30 parts by weight of vinylidene chloride are mixed thoroughly thereby forming a stable emulsion. The mixture is polymerized in 1 to 24 hours thereby producing a poly(sodium silicate-vinylidene chloride copolymer emulsion).