Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Toluene | HCID 1140 | — |
| Reactant | Titanium Tetrachloride | HCID 24193 | — |
| Product | HCID 87097284 | HCID 87097284 | — |
Reaction Steps
To the solid component mentioned above, 40 ml of toluene was added and titanium tetrachloride was added in an amount calculated to give a volumetric titanium tetrachloride/toluene ratio of 3/2. The resultant combined liquid was heated to 90° C. The hot mixture was kept stirred and a mixed solution of 2 ml of di-n-butyl phthalate and 5 ml of toluene was added dropwise to the hot mixture over a period of 5 minutes. The resultant mixture was stirred at 120° C. for 2 hours. The solid product consequently obtained in the mixture was separated by filtration and washed at 90° C. two times each with 100 ml of toluene. Further, the washed solid product and titanium tetrachloride added thereto in an amount calculated to give a volumetric titanium tetrachloride/toluene ratio of 3/2 were stirred at 120° C. for 2 hours. The solid substance consequently formed therein was separated by filtration at 110° C. and washed seven times each with 100 ml of n-hexane at room temperature, to obtain 5.5 g of a catalyst component.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04950630 |
|---|
| Source dataset | uspto-grants-1990_08 |
|---|
| ORD ID | ord-ce48eb23db8c45df873df6f9fd4135d2 |
|---|
| Source note | uspto-grants-1990_08 |
|---|