Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Benzoyl Peroxide | HCID 7187 | — |
| Reactant | Lauryl Methacrylate | HCID 8906 | — |
| Reactant | Crotonic Acid | HCID 637090 | — |
| Product | HCID 86747973 | HCID 86747973 | — |
Reaction Steps
To the above solvent, a mixture of 200 g of lauryl methacrylate, 3 g of crotonic acid and 1 g of benzoyl peroxide was added dropwise at a constant speed over a period of 2 hours, followed by stirring at 90° C. for 3 hours to complete the polymerization reaction. Thus, lauryl methacrylate - crotonic acid copolymer was obtained.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US05328794 |
|---|
| Source dataset | uspto-grants-1994_07 |
|---|
| ORD ID | ord-61d7e4b416e945129f8312493b347c53 |
|---|
| Source note | uspto-grants-1994_07 |
|---|