Procedure
To 15g. of styrene placed in a tube is added 5g. of the product obtained on Example V. The tube is sealed under a nitrogen atmosphere and heated for 7 hours at +70° C to +100° C. The polymer obtained from the reaction is dissolved in benzene and precipitated with odorless mineral spirit. The polymer is dried in a vacuum oven for sixteen hours at +50° C and tested by the demixing test. (4)-(5).
Workup
- customof the product obtained on Example V
- customThe tube is sealed under a nitrogen atmosphere
- temperatureheated for 7 hours at +70° C to +100° C
- customThe polymer obtained from the reaction
- customprecipitated with odorless mineral spirit
- customThe polymer is dried in a vacuum oven for sixteen hours at +50° C