Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1730434Generated: October 26, 2026

Sulfuric Acid → Tetramethylthiuram disulphide water

https://huagongshe.com/reaction/1730434

Reaction equation

Participants

RoleNameHCIDCharge
ReactantSulfuric AcidHCID 1118—
ReactantThiramHCID 5455—
SolventWaterHCID 962—
ProductTetramethylthiuram disulphide waterHCID 86734189—

Reaction Conditions

Temperature55 °C

Reaction Steps

A tetramethylthiuram disulphide water slurry was prepared by mixing 160 parts of water with 24 parts of tetramethylthiuram disulphide powder in a flask. The slurry was made acidic to litmus paper by the addition of a fewdrops of concentrated sulphuric acid. The slurry was then heated to about 55° C. at atmospheric pressure and continuously stirred to maintaina good suspension.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS03992448
Source datasetuspto-grants-1976_11
ORD IDord-7b042347ff04494da91f6f7d53b9c43c
Source noteuspto-grants-1976_11