Formaldehyde → Crl-8131

https://huagongshe.com/reaction/1732834

Reaction equation

Participants

RoleNameHCIDCharge
ReactantFormaldehydeHCID 712—
ReactantSulfuric AcidHCID 1118—
ReactantUreaHCID 1176—
ReactantTriethanolamineHCID 7618—
ReactantCrl-8131HCID 24751—
ReactantSorbitan mono-(9Z)-9-octadecenoateHCID 9920342—
ReactantSpan #80 (Sorbitan monooleate)HCID 70693544—
ReactantHCID 178435162HCID 178435162—
CatalystTitanium oxide (Ti3O)HCID 162651—
SolventWaterHCID 962—
SolventO-XyleneHCID 7237—
ProductCrl-8131HCID 24751—
ProductUrea formaldehyde foamHCID 62705—

Reaction Steps

A urea-formaldehyde prepolymer solution is prepared by heating an aqueous solution of two-hundred-twenty grams of 37% formaldehyde and eighty-two grams of urea, adjusted to pH 8 with triethanolamine, at 70° C. for one hour. Fifty grams of this prepolymer solution are mixed with thirty grams of a 50% by weight dispersion of titanium dioxide in distilled water, and adjusted to pH 6 with dilute sulfuric acid. The aqueous dispersion is emulsified in a solution of six grams of Pluronic L 122, three grams of sorbitan monooleate (commercially available as Span 80 from ICI America) and 1.5 grams of a poly(oxyethylene)-poly(oxypropylene) block copolymer with 30% poly(oxyethylene) and a molecular weight of about 2500 (commercially available as Pluronic L 63) in one-hundred grams of xylene to yield a water-in-oil emulsion. This is treated with four milliliters of a 50% by weight solution of monobutyl acid phosphate in toluene and stirred for two hours.