関与物質
| 役割 | 名称 | HCID | 仕込み量 |
|---|
| 反応物 | Ethylene Oxide | HCID 6354 | — |
| 反応物 | Methacrylamide | HCID 6595 | — |
| 反応物 | Ethyl Acrylate | HCID 8821 | — |
| 反応物 | Potassium Persulfate | HCID 24412 | — |
| 反応物 | Methylolmethacrylamide | HCID 70208 | — |
| 反応物 | Butanedioic acid, 2-methylene-, sodium salt (1:2) | HCID 79326 | — |
| 反応物 | Sodium | HCID 5360545 | — |
| 反応物 | Triisobutylphenol | HCID 22253180 | — |
| 溶媒 | Water | HCID 962 | — |
| 生成物 | Ethylene Oxide | HCID 6354 | — |
| 生成物 | 2-Isononylphenol | HCID 119757 | — |
反応手順
0.2 part by weight of the sodium salt of a sulfated addition product of triisobutylphenol and 7 mols of ethylene oxide (emulsifier A) and 0.02 part by weight of potassium peroxodisulfate are dissolved in 61.5 parts by weight of completely desalted water at 80° C. in a polymerization vessel provided with a reflux condenser, stirrer, thermometer, and feed vessel. An emulsion, earlier prepared from 83 parts by weight of ethyl acrylate, 10 parts by weight of methoxy polyethyleneglycol methacrylate [formula (I), n=15], 5 parts by weight of disodium itaconate, 1.2 parts by weight of N-hydroxymethyl methacrylamide, 0.8 part by weight of methacrylamide 2.3 parts by weight of emulsifier A, 1 part by weight of the addition product formed between isononylphenol and 100 mols of ethylene oxide (emulsifier B), 0.18 part by weight of potassium peroxodisulfate, and 94 parts by weight of desalted water, is added dropwise to this solution at 80° C. over a period of 4 hours. After addition is complete, the reaction temperature is kept for one further hour at 80° C. and subsequently the mixture is cooled to room temperature. A coagulate-free dispersion having a solids content of about 40% is obtained.
情報源と証拠
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 特許番号 | US04239671 |
|---|
| 出典データセット | uspto-grants-1980_12 |
|---|
| ORD ID | ord-2b8cf098b82d4c30bc5d7382360019ec |
|---|
| 出典メモ | uspto-grants-1980_12 |
|---|