HRID1741562

反应详情

EQUATION

反应方程式

HRID 1741562 的结构方程式

PROCEDURE

实验过程

Styrene methacrylic acid copolymer was prepared by using the same procedures as in Example 1 except 67 parts of styrene and 3 parts of methacrylic acid was used in place of 70 parts of styrene. The resulting copolymer had a number average molecular weight of 3,800, a glass transition temperature of 70° C., and a non-volatile content of 99.8%.