| Role | Name | HCID | Charge |
|---|
| Reactant | Cyclopentadiene | HCID 7612 | — |
| Reactant | Butyllithium | HCID 178418339 | — |
| Catalyst | Zirconium chloride (ZrCl4), (T-4)- | HCID 9856075 | — |
| Product | n-Butyl cyclopentadiene | HCID 102598 | — |
Reaction Steps
n-Butylcyclopentadiene was prepared analogously to Example 1 and freed or inorganic salts and excess cyclopentadiene. The solution so obtained was cooled to 0° C. and subsequently admixed dropwise with 9.7 g of n-butyllithium (90% strength in hexane; 136 mmol). The mixture was allowed to react for a further 30 minutes while stirring. 15.8 g of ZrCl4 (68 mmol) was added at 0°-10° C. and the mixture was stirred for 2 hours at room temperature.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US05336795 |
|---|
| Source dataset | uspto-grants-1994_08 |
|---|
| ORD ID | ord-b35ca5e4f3d54c11a93ceda210a1394b |
|---|
| Source note | uspto-grants-1994_08 |
|---|