Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Benzoyl Peroxide | HCID 7187 | — |
| Reactant | Indole-3-Butyric Acid | HCID 8617 | — |
| Reactant | 2-Hydroxyethyl Methacrylate | HCID 13360 | — |
| Solvent | Ethyl Acetate | HCID 8857 | — |
| Product | HCID 131724103 | HCID 131724103 | — |
Reaction Steps
In a glass polymerization bottle were charged 80 g IOA, 18 g IBA, 2 g HEMA, 100 g ethyl acetate, and 0.5 g dibenzoyl peroxide. The bottle was purged with nitrogen, sealed, and tumbled in a water bath maintained at 60° C. for 14 hrs. The resulting terpolymer, IOA/IBA/HEMA, was isolated by precipitation in petroleum ether. The terpolymer has a number average molecular weight of 180,000 (polymer V). This high molecular weight polymer having a pendent hydroxyl moiety was mixed with the low molecular weight oligomer composition used in Example 15 in Table 4, coated onto a PET liner, and subjected to 80° C. to affect crosslinking, as in Examples 7–15. Properties of the resulting crosslinked polymer are shown in Table 5.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US07015286B2 |
|---|
| Source dataset | uspto-grants-2006_03 |
|---|
| ORD ID | ord-491d47a4e4da4122850b4c41becb2565 |
|---|
| Source note | uspto-grants-2006_03 |
|---|