Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1759238Generated: November 1, 2026

Styrene → Alpha-Methylstyrene

https://huagongshe.com/reaction/1759238

Reaction equation

Participants

RoleNameHCIDCharge
ReactantStyreneHCID 7501—
ReactantAcrylonitrileHCID 7855—
ReactantAntimony TrioxideHCID 14794—
ReactantSilicaHCID 24261—
ReactantStibanalHCID 6327673—
ProductAlpha-MethylstyreneHCID 7407—
ProductAcrylonitrileHCID 7855—
ProductStibanalHCID 6327673—

Reaction Steps

An aqueous colloidal dispersion of antimony oxide sold by Nyacol, Inc., Ashland, Mass. under the trade name Nyacol A-1530, containing 30 weight percent antimony oxide was added to an aqueous anionic latex containing 40 weight percent of polybutadiene grafted with 20 parts of an interpolymer containing 70 percent styrene and 30 percent acrylonitrile per 100 parts of polybutadiene and was stirred to provide a uniform blend. The procedure of Example 1 was then carried out to obtain a blend of rubber-occluded antimony oxide in an interpolymer of α-methylstyrene and acrylonitrile. The ratio of styrenic interpolymer to (ungrafted) polybutadiene to colloidal antimony oxide was 22:8:1.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04339556
Source datasetuspto-grants-1982_07
ORD IDord-9c00261984db41f09818dda44c957a26
Source noteuspto-grants-1982_07