Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Styrene | HCID 7501 | — |
| Reactant | Dibutyl maleate | HCID 5271569 | — |
| Catalyst | Di-tert-butyl peroxide | HCID 8033 | — |
| Product | HCID 10359426 | HCID 10359426 | 93% |
Reaction Steps
Into a 1 liter four-necked flask, 228 g (1 mol) of dibutyl maleate was charged and heated to 160° C. under a nitrogen stream. Then, a mixture comprising 104 g (1 mol) of styrene and 8.76 g (0.06 mol) of di-tert-butyl peroxide, was continuously dropwise added thereto under stirring over a period of 5 hours. After the addition, the mixture was further reacted at the same temperature for 1 hour. After the completion of the reaction, low boiling point components and unreacted monomers contained in the reaction mixture were removed by distillation under a reduced pressure of from 1 to 3 mmHg, to obtain 309 g (yield: 93%) of a styrene-dibutyl maleate copolymer.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04828720 |
|---|
| Source dataset | uspto-grants-1989_05 |
|---|
| ORD ID | ord-a36165816a2944c39234f77a997bdd96 |
|---|
| Source note | uspto-grants-1989_05 |
|---|