Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Hexane | HCID 8058 | — |
| Solvent | Water | HCID 962 | — |
| Product | 1-Decene | HCID 13381 | — |
Reaction Steps
To a 250 ml high pressure kettle for polymerization, 80 ml of n-hexane, 8 g of catalyst obtained as above, 30 ml of 1-decene and 0.174 ml of water as a co-catalyst are added. 1-decene oligomerization is carried out under a condition of a temperature of 80° C. and a pressure of 1.0 MPa for 5 hours, after which the reaction is stopped and the catalyst is filtered out, the solvent n-hexane is removed by distillation under ambient pressure, and then unreacted monomer 1-decene and part of the dimers are removed by distillation under reduced pressure to produce the final oligomer. The conversion of 1-decene is 54.1 wt %. The oligomer has a kinematic viscosity at 40° C. of 16.51 mm2/s, a kinematic viscosity at 100° C. of 5.81 mm2/s and a viscosity index of 208.80.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US09248430B2 |
|---|
| Source dataset | uspto-grants-2016_02 |
|---|
| ORD ID | ord-861ecfa810ce4d1799c57abc1bd6266d |
|---|
| Source note | uspto-grants-2016_02 |
|---|